Brief Introduction of Metal Wire
for thermal spray coating:Wire Specification:
usage | List | Name | Main ingredient | Coating performance |
Wear-resistant | SX-801 | SX-HCrC | Cr3C2,Cr,C,Mn,Fe,V,Mo | Good high-temperature resistant Good erosion resistant Good high temperature oxidation resistant, hardness≥HRC52, working temperature: 800ºC |
SX-802 | SX-HCrCA | Cr3C2,Cr,C,Ti,Ni,Nb,Tombarthite | austenite structure good high-temperature resistant good erosion resistant good high temperature oxidation resistant, hardness≥HRC55 working temperature: 1000ºC |
SX-803 | SX-TiAlA | TiAl,Cr3C2,C,V,Mn,Nb,Al,Fe | Good high-temperature resistant Good erosion resistant Good high temperature oxidation resistant Good high temperature corrosive resistant hardness≥HRC48 working temperature: 1200ºC amorphous state |
SX-804 | SX-7Cr13 | Cr,C,Fe,V,Mn,Si,B | Good wear-resistant hardness≥HRC50 working temperature:600ºC no need for base coating bonding strength≥40MPa |
SX-805 | SX-7Cr13A | Cr,C,Ni,Ti,Nb,Fe | Good wear-resistant A bit of oxidation resistant hardness≥HRC50 working temperature: 700ºC no need for base coating bonding strength≥40MPa |
SX-806 | SX-3Cr13 | Cr,C,Fe,Mn,V,Si,B | normal wear-resistant and oxidation resistant good ductility hardness≥HRC38 working temperature: 600ºC no need for base coating bonding strength≥40MPa |
SX-807 | SX-13Cr13 | Cr,C,Fe,Mn,Mo,V,Si,B | good wear-resistant normal oxidation resistant high friability hardness≥HRC48 working temperature: 600ºC |
Anti-corrosion | SX-601 | SX-HCr | Cr,C,Cr3C2,V,Al,Fe | Good Sulfur corrosion resistant Good high temperature oxidation resistant good wear-resistant |
SX-602 | SX-HCrA | Cr,C,Cr3C2,Ni,Nb,Ti,Tombarthite | austenite structure Good Sulfur corrosion resistant Good high temperature oxidation resistant good wear-resistant hardness≥HRC50 working temperature: 1200ºC |
SX-603 | SX-TiAlB | TiAl3,Cr3C2,C,V,Mo,Nb,Al,Fe | Good high temperature oxidation resistant Good high temperature wear-resistant hardness≥HRC48 working temperature: 1200ºC amorphous state |
SX-604 | SX-TiAlC | TiAl3,Ti3Al,Cr,C,Ni,Ti,Nb,Tombarthite | austenite structure good performance in high temperature Good high temperature oxidation resistant Good high temperature corrosion resistant hardness≥HRC48 working temperature: 1300ºC |
Ultra -hard | SX-301 | SX-NiCrBSiY | Ni,Cr,Cr3C2,Ti,C,B,Si,Y | austenite structure fine and close coating good wear-resistant good performance in medium and high temperature hardness≥HRC56 |
SX-302 | SX-FeCrBSi | Cr,C,B,Si,Mo,V,Fe | ferrite structure fine and close coating good wear-resistant good performance in medium and high temperature hardness≥HRC55 |
SX-303 | SX-WC | WC,Ni,Cr,C,B,Si,Fe | High hardness Good wear-resistant Substitution of flame WC spraying good performance in medium and high temperature hardness≥HRC58 |
SX-304 | SX-MeO | Ni-Al2O3,Cr2O3,TiC,Cr,Ti,Fe | Ceramic coating High hardness Good wear-resistant good performance in high temperature hardness≥HRC68 |
Nano | SX-401 | SX-N-WC | Ni-WC(Nano),Cr,C,Ni,Fe | Nano coating Fine and smooth Low porosity rate High hardness High wear-resistant working temperature: 800ºC hardness≥HRC60 |
SX-402 | SX-N-AlO | Ni-Al2O3(Nano),Cr2O3,TiAl3,Cr,Ni,C,Fe | Nano coating Ceramic structure High hardness Good high temperature oxidation resistant thin coating will be better hardness≥HRC65 |
SX-403 | SX-N-TiC | Ni-TiC(Nano),TiAl3,Cr,C,Ni,Fe | Nano coating Ceramic structure Fine and close coating Good performance in high temperature Good hardness hardness≥HRC68 |
SX-404 | SX-N-MeO | Ni-Al2O3-TiC(Nano),Cr2O3,Cr,Ti,C,Ni | Nano coating austenite structure Ceramic structure High-temperature resistant oxidation resistant hardness≥HRC69 |
Base coating (used for better bonding strength) | SX-501 | SX-Ni-Al | Tegmen material:Ni cored material:Al | Good high temperature oxidation resistant Good high temperature corrosion resistant bonding strength≥55MPa |
SX-502 | SX-Ni-Al-Ti | Tegmen material: Ni cored material:Al,Ti | For base coating Stable performance Better high temperature oxidation and corrosion resistant bonding strength≥60MPa |
SX-503 | SX-Al-Ni | Tegmen material: Al cored material:Ni | Special base coating material Better corrosion resistant under medium temperature Used for non-ferrous metal matrix bonding strength≥50MPa |
Arc Spraying Solid Wires
usage | List | Name | Main ingredient | Coating performance |
High temperature oxidation and corrosion resistant | SX-101 | SX-NiCrTi(45CT) | Ni,Cr,Ti | Fine, close and smooth coating Good high temperature oxidation resistant Good Sulfur corrosion resistant bonding strength≥40MPa hardness≥HRC38 working temperature:1400ºC |
SX-102 | SX-NiCr | Ni,Cr | Good high temperature oxidation resistant Good high temperature corrosion resistant Smooth coating structure bonding strength≥40MPa hardness≥HRC32 working temperature:1200ºC |
SX-103 | SX-NiCrAl | Ni,Cr,Al | Fine and smooth coating Good high temperature oxidation resistant Good high temperature corrosion resistant Stable performance in high temperature bonding strength≥45MPa hardness≥HRC35 working temperature:1200ºC |
SX-104 | SX-FeCrAl | Cr,Al,Fe | Good oxidation resistant under medium and high temperature Normal Sulfur corrosion resistant Big friability for the coationg hardness≥HRC38 working temperature:900ºC |
SX-105 | SX-304 | Cr,Ni,Ti,Fe | austenite structure matrix big expansion coefficient Good oxidation resistant under medium and high temperature Good ductibility Low hardness working temperature:800ºC |
SX-106 | SX-316 | Cr,Ni,Ti,Fe | austenite structure big expansion coefficient Good high temperature oxidation resistant Good ductibility Low hardness working temperature: 1000ºC |
Wear-resistant | SX-201 | SX-1Cr13 | Cr,C,Ni,Mo,V,Mn,Fe | Ferrite matrix A bit oxidation resistant under medium temperature Good ductibility for the coating Low hardness hardness≥HRC30 working temperature: 700ºC |
SX-202 | SX-2Cr13 | Cr,C,Ni,Mo,V,Mn,Fe | Ferrite matrix A bit oxidation resistant under medium temperature Good collocation of ductibility and hardness hardness≥HRC35 working temperature: 700ºC |
SX-203 | SX-3Cr13 | Cr,C,Ni,Mo,Mn,V,Fe | Ferrite matrix A bit oxidation resistant under medium temperature Normal ductibility Good wear-resistant |
SX-204 | SX-4Cr13 | Cr,C,Ni,Mo,V,Mn,Fe | Ferrite matrix A bit oxidation resistant under medium temperature Good wear-resistant Big friability for the coationg hardness≥HRC42 working temperature: 700ºC |
SX-205 | SX-60SiMn | C,Mn,Si,Cr,Fe | Good wear-resistant under low and medium temperature Big friability for the coationg hardness≥HRC45 |
SX-206 | SX-50CrV | C,Cr,V,Si,Mn,Fe | Good wear-resistant under low and medium temperature Normal ductibility hardness≥HRC45 |
Base coating | SX-301 | SX-NiAl | Ni,Al | exothermic reaction Micro metallurgical structure Smooth coating Good oxidation and corrosion resistant bonding strength≥60MPa working temperature: 1000ºC |
SX-302 | SX-NiAlTi | Ni,Al,Ti | Strong exothermic reaction Good micro osmosis for the bonding surface Micro metallurgical structure Good oxidation and corrosion resistant Stable performance under high temperature bonding strength≥70MPa working temperature: 1200ºC |
non-ferrous metal | SX-401 | SX-Al | Al | Good corrosion resistant for air, water, concentrated nitric acid, nitrate, Organic medium Good heat and electric conduction ability |
SX-402 | SX-AlZn | Al,Zn,Mg | stress corrosion resistant good thermal deformation ability strong intensity fine and close coating |
SX-403 | SX-AlSi | Al,Si,Mg | Good plasticity Air corrosion resistant Can be heat tinting |
SX-404 | SX-Cu | Cu | Good electric conduction and electric heating performance Good ductility Corrosion resistant for air, organic acid, alkali, salt good printing ink adsorption ability |
SX-405 | SX-CuZn | Cu,Zn | Good electric conduction and electric heating performance Corrosion resistant for air, salt Fine and smooth coating High hardness |
SX-406 | SX-CuNiAl | Cu,Ni,Al | Good electric conduction and electric heating performance Good wear-resistant and erosion resistant ability Good heat-resistant ability |
SX-407 | SX-Zn | Zn | Low melting point Easy to spray Dry atmosphere corrosion resistant Can be used as anode coating to protect matrix metal |
Features: Nickel Aluminium base material for first stage of arc spraying process.
Our cases:
Package & Delivery
Package: Carton Package
Weight: Pending
Size: Pending
Delivery Time
Within 10 days after deposit settled.
Payment method:
100% T/T payment.
Products you may be interested in as well:
▪ Metal Powder For Thermal Spray Coating
▪ HVOF Flame Spraying Machine
▪ Plasma Spray Machine
▪ Arc spray equipment
▪ High power flame spray plastic equipment
▪ Spraying auxilliary equipment such as spraying booth
▪ Peripheral equipment such as sand blasting machine
▪ Coating performance testing equipment
▪ We also provide worldwide thermal coating service.
Our Service:
Pre-order
1.We will offer fast reply on your enquiry.
In-order
1.We will keep you updated with professional customer service
2.Package and transport products strictly accordance with export standard.
After-order
1.We supply the customs clearance for you and we will help you if you have special requests.
2.Under the premise of correct installation normal maintenance and using. 12 month warranty.
3.During the course of installation and adjustment, we will process followup after-sale service by communicating with customers, offering free training, etc.
4.Lifelong free technical support.
FAQ
Question:What does your machine do?
Answer: Our machine is for surface treatment.
Question:Do you offer any technical support such as training for the machine operation?
Answer: Yes, we do. We offer training for free.
Question:Do you offer the coating service besides machine?
Answer: Yes,we can offer the coating service around the world. Option 1 is that you send the workpiece to our factory and we spray it in the plant. Option 2 is that we send our workers to where the workpiece is and spray at the spot.
About Our Company
Since 1978, with two generations for about 30 years, Sanxin Metal has been dedicated to thermal spray projects. Now we are a famous company in surface engineering in China, and acquire great success in industries like electric power, bridge, municipal building, papermaking and printing, petroleum, chemical engineering, metallurgy, etc. Now we have completed more than 50 projects in anticorrosive coating and 250 projects in boiler spraying of generating station with construction areas over 4,500,000sqm. Our company has 13 experienced and qualified construction groups and more than 150 skilled workers. We have more than 50 sets of TAFA supersonic arc spray equipment and plasma spray equipment that are imported from America, and more than 30 sets of powerful air compressors, sand sprayers and air dusting machines. We also have more than 10 complete sets of advanced quality detecting equipment, coating surface analyzing devices, large scale lathes and high precise grinders.
In past 30 years, we also focus on High-frequency induction heating equipment, intermediate frequency electric furnace, CNC quenching machine, non-standard induction heating equipment. We accumulated much experience in special sensorsa and a wide range of technology solutions, solved hundreds of high-grade, special, tricky technical problems.
Company qualification
Sanxin Metal is a member of China Surface Engineering Association and national thermal spray collaboration. We have thermal spray engineering construction authoritative qualification and ISO9001:2000 Quality accreditation system certification. During our 30 plus years of business, we have always been devoting ourselves to developing, researching and manufacturing more efficient, durable and reliable products to satisfy our customers.
Company value
Today, as throughout our history, our customers challenge us to provide surface solutions and heating treatment solutions that will help them improve the value and service performance of the components they produce or require for their own operations. We have been dedicated to earn their loyalty since the beginning through commitment, service and innovation that will keep our customers at the forefront of their fields by providing the advantages they need in today and in the future competitive climate.
Our vision
To be the best performing surface solution and induction heating company in China and in the world as determined by our customers, employees, suppliers and the communities in which we operate.